{"id":302472,"date":"2024-10-19T20:39:55","date_gmt":"2024-10-19T20:39:55","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/bs-iso-212072015\/"},"modified":"2024-10-25T18:11:20","modified_gmt":"2024-10-25T18:11:20","slug":"bs-iso-212072015","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/bsi\/bs-iso-212072015\/","title":{"rendered":"BS ISO 21207:2015"},"content":{"rendered":"
This International Standard defines two accelerated corrosion test methods to be used in assessing the corrosion resistance of products with metals in environments where there is a significant influence of chloride ions, mainly as sodium chloride from a marine source or by winter road de-icing salt, and of corrosion-promoting gases from industrial or traffic air pollution.<\/p>\n
This International Standard specifies both the test apparatus and test procedures to be used in executing the accelerated corrosion tests.<\/p>\n
The methods are especially suitable for assessing the corrosion resistance of sensitive products with metals, e.g. electronic components, used in traffic and industrial environments.<\/p>\n
PDF Pages<\/th>\n | PDF Title<\/th>\n<\/tr>\n | ||||||
---|---|---|---|---|---|---|---|
6<\/td>\n | Foreword <\/td>\n<\/tr>\n | ||||||
7<\/td>\n | Introduction <\/td>\n<\/tr>\n | ||||||
9<\/td>\n | 1\tScope 2\tNormative references 3\tApparatus and reagents <\/td>\n<\/tr>\n | ||||||
10<\/td>\n | 4\tEvaluation of the corrosivity of the tests 4.1\tReference test panels <\/td>\n<\/tr>\n | ||||||
11<\/td>\n | 4.2\tArrangement of the reference panels during testing 4.3\tDetermination of mass loss after testing 4.4\tSatisfactory performance of test <\/td>\n<\/tr>\n | ||||||
12<\/td>\n | 5\tTest objects 6\tProcedure 6.1\tTest method A 6.1.1\tTest cycle 6.1.2\tSalt spray testing followed by drying (step a) <\/td>\n<\/tr>\n | ||||||
13<\/td>\n | 6.1.3\tExposure to corrosive gases followed by drying (step b) 6.1.4\tTest duration 6.2\tTest method B 6.2.1\tTest cycle <\/td>\n<\/tr>\n | ||||||
14<\/td>\n | 6.2.2\tSalt spray testing followed by drying (step a or step c) 6.2.3\tExposure to corrosive gases (step b or step d) 6.2.4\tTest duration 7\tEvaluation of results <\/td>\n<\/tr>\n | ||||||
15<\/td>\n | 8\tTest report <\/td>\n<\/tr>\n | ||||||
16<\/td>\n | Annex\u00a0A (informative) Recommended test periods <\/td>\n<\/tr>\n | ||||||
17<\/td>\n | Bibliography <\/td>\n<\/tr>\n<\/table>\n","protected":false},"excerpt":{"rendered":" Corrosion tests in artificial atmospheres. Accelerated corrosion tests involving alternate exposure to corrosion-promoting gases, neutral salt-spray and drying<\/b><\/p>\n |