ASTM-A608 1998
$40.63
A608-91a(1998) Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures
Published By | Publication Date | Number of Pages |
ASTM | 1998 | 5 |
ASTM A608-91a-Reapproved1998
Historical Standard: Standard Specification for Centrifugally Cast Iron-Chromium-Nickel High-Alloy Tubing for Pressure Application at High Temperatures
ASTM A608
Scope
1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.
1.2 The grades of high alloys detailed in Table 1 are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.
1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.
1.4 The values stated in inch-pound units are to be regarded as the standard.
Keywords
centrifugal casting; pressure containing parts; steel tube; alloy; temperature service applications, high
ICS Code
ICS Number Code 23.040.10 (Iron and steel pipes)