ASME QG2 WLD 2009
$50.05
ASME QG2-WLD-2009
Published By | Publication Date | Number of Pages |
ASME | 2009 | 154 |
PDF Catalog
PDF Pages | PDF Title |
---|---|
4 | A Quick Guide to Welding and Weld Inspection |
6 | Contents |
9 | Foreword by Series Editor |
11 | Introduction |
13 | A 10 Minute Guide |
16 | Chapter 1 Abbreviations, Terminology andWelding Symbols Abbreviations |
17 | Common terms Joint terminology Weld terminology |
28 | Supplementary information Other common rules |
32 | Chapter 2 Duties of a Welding Inspector Before welding |
34 | During welding After welding |
35 | Repairs |
37 | Chapter 3 Analysis of a Fusion Weld Components of a welded joint |
39 | What makes a good fusion weld? |
41 | Weld joint: preparation methods |
42 | Weld joint: shape Residual stress and distortion |
47 | Minimising stresses and distortion |
51 | Chapter 4 Materials and Their Weldability Carbon equivalency |
52 | Classification of steels |
53 | Alloying elements |
58 | Material properties |
59 | Heat treatment of steels |
64 | Chapter 5 Welding Processes Manual metal arc (MMA)/shielded metal arcwelding (SMAW) |
68 | Metal inert gas (MIG)/metal active gas (MAG)/gasmetal arc welding (GMAW) |
74 | Flux-cored arc welding (FCAW) |
76 | Tungsten inert gas (TIG)/gas tungsten arcwelding (GTAW) |
78 | Submerged arc welding (SAW) |
82 | Chapter 6 Non-destructive and DestructiveTesting Liquid penetrant testing (PT) |
84 | Magnetic particle testing (MT) |
86 | Ultrasonic testing (UT) |
88 | Radiographic testing (RT) |
92 | Tension tests Bend tests |
93 | Charpy tests |
96 | Hardness testing |
98 | Macro samples |
100 | Micro samples Fillet fracture test Butt weld fracture test (nick break) |
103 | Chapter 7 Fracture Modes and Welding Defects Imperfection categories Hydrogen-induced cold cracking (HICC) |
105 | Solidification cracking |
108 | Reheat cracking Lamellar tearing |
112 | Weld decay |
113 | Porosity |
116 | Solid inclusions Lack of fusion |
117 | Incomplete root penetration Root concavity |
118 | Excessive root penetration Overlap |
119 | Underfill Undercut |
120 | Crater pipe |
121 | Burn-through Root oxidation |
122 | Spatter Magnetic arc blow |
123 | Chapter 8 Codes, Standards and Documentation |
126 | The PED and UK PER |
128 | Welding procedure qualifications |
129 | Procedure qualification record (PQR) Welding procedure specification (WPS) |
132 | Welder qualifications |
140 | Chapter 9 Health and Safety Health and Safety at Work Act |
141 | Electrical safety |
142 | Welding/cutting process safety |
143 | Personal protective equipment (PPE) |
145 | COSHH and workplace exposure limits (WEL) |
147 | Lifting equipment/pressure system requirements |
148 | Hand tools and grinding machines Other precautions before welding starts Causes of accidents |
149 | Permit-to-work Tanks and drums |
150 | Index |