{"id":302324,"date":"2024-10-19T20:39:12","date_gmt":"2024-10-19T20:39:12","guid":{"rendered":"https:\/\/pdfstandards.shop\/product\/uncategorized\/bs-en-754-22013\/"},"modified":"2024-10-25T18:09:58","modified_gmt":"2024-10-25T18:09:58","slug":"bs-en-754-22013","status":"publish","type":"product","link":"https:\/\/pdfstandards.shop\/product\/publishers\/bsi\/bs-en-754-22013\/","title":{"rendered":"BS EN 754-2:2013"},"content":{"rendered":"
This European Standard specifies the mechanical property limits resulting from tensile testing applicable to aluminium and aluminium alloy cold drawn rod\/bar and tube.<\/p>\n
Technical conditions for inspection and delivery, including product and testing requirements, are specified in EN 754-1. Temper designations are defined in EN 515. The chemical composition limits for these materials are given in EN 573-3.<\/p>\n
PDF Pages<\/th>\n | PDF Title<\/th>\n<\/tr>\n | ||||||
---|---|---|---|---|---|---|---|
6<\/td>\n | 1 Scope 2 Normative references 3 Mechanical property limits 3.1 General 3.2 Elongation <\/td>\n<\/tr>\n | ||||||
7<\/td>\n | 3.3 Reference list of the tables of mechanical properties of the relevant aluminium and aluminium alloys <\/td>\n<\/tr>\n | ||||||
8<\/td>\n | 3.4 Detailed tables of mechanical properties <\/td>\n<\/tr>\n | ||||||
45<\/td>\n | Annex A (informative) List of tempers used in Tables 1 to 37 <\/td>\n<\/tr>\n<\/table>\n","protected":false},"excerpt":{"rendered":" Aluminium and aluminium alloys. Cold drawn rod\/bar and tube – Mechanical properties<\/b><\/p>\n |